Your layer thickness is set at 0.5, for 50 microns it should be 0.05.

Try running the Kudo calibration model a few times at different exposures to dial in your exposure setting.

https://www.dropbox.com/s/3b4rjogjcsat41g/KudoCalibrationSample.stl?dl=0

When I ran this with Spot HT I found around 4 seconds worked for me. I have attached my settings

For my models I usually have a 0.2mm base thickness with 60 seconds for first layer then 30 seconds for next 3.

It is also better to be a bit conservative on the lift speeds, after some issues with warping trays using 3DM Cast I have gone back to 15mm / min for all layers. You can reduce the lift height a little bit to compensate if your prints start taking too long.

  • This reply was modified 3 hours, 44 minutes ago by  Peter.
Attachments:
You must be logged in to view attached files.

Viewing all articles
Browse latest Browse all 1661

Latest Images

Trending Articles



Latest Images